The OEM flexographic plate supply is one of the world’s leading manufacturers in digital and conventional formats, these products can compete with the top brands you ever used before, yet at an affordable price.
In the corrugated industry, typically there are two types of applications, one is the corrugated board printing which uses plates in thickness from 2.84mm to 7.0mm, and the other one is pre-print liner which uses plates in thickness as thin as 1.14mm. These flexographic printing plates are compatible with all Water-based and Alcohol-based inks, and certain UV, yet we urge you to test before using for specific application of Solvent-based inks.
The most general sizes available are:
- 2032mm * 1270mm
- 2032mm * 1067mm
- 1524mm * 1067mm
- 1016mm * 762mm
We can supply both Digital Plates and conventional Analogue Plates, plus plate making equipment from Exposure, Wash-out, Dyer Drawer to Solvent Recycle, you can view more about all of these items on our website for your total print requirements.
Specification of print plates typically for corrugated sheet |
||||||||||||
Model |
C700-Ⅱ | C635L | C550L | C470 | C394 | C394-Ⅱ | C394-Ⅲ | C394Q-Ⅱ | C318L | C284-Ⅱ | C284L |
C284 |
Thickness/mm |
7.00 | 6.35 | 5.50 | 4.70 | 3.94 | 3.94 | 3.94 | 3.94 | 3.18 | 2.84 | 2.84 | 2.84 |
Hardness/Shore A |
38-40 | 36-38 | 36-38 | 36-38 | 43 | 43 | 36-38 | 39-42 | 37 | 46 | 38-40 | 42-45 |
Relief depth/mm |
3.2-3.8 |
2.2-3.0 | 2.0-3.0 | 1.2-2.2 | 1.8-2.0 | 1.8-2.0 | 1.8-2.0 | 1.8-2.0 | 0.9-1.5 | 1.0-1.4 | 1.0-1.4 |
1.0-1.4 |
Dot reproduction/% |
3-95% | 3-95% | 3-95% | 3-95% | 3-95% | 3-95% | 3-95% | 3-95% | 2-95% | 2-95% | 2-95% |
2-95% |
Line/lpi |
85 | 85 | 85 | 85 | 100 | 100 | 100 | 100 | 120 | 120 | 120 |
120 |
Isolated line/down to mm |
0.30 | 0.30 | 0.30 | 0.30 | 0.30 | 0.30 | 0.30 | 0.30 | 0.175 | 0.175 | 0.175 |
0.175 |
Isolated dot/down to mm |
0.50 | 0.50 | 0.50 | 0.50 | 0.50 | 0.50 | 0.50 | 0.50 | 0.25 | 0.25 | 0.25 |
0.25 |
Back Exposure/Sec |
180-280 | 160-280 | 80-220 | 80-220 | 35-70 | 35-70 | 50-70 | 25-40 | 25-75 | 25-40 | 25-50 |
10-30 |
Main Exposure/min |
16-24 | 16-24 | 10-20 | 10-20 | 8-20 | 8-20 | 8-20 | 8-20 | 8-20 | 8-20 | 8-15 |
8-15 |
Rinsing/min |
10-12 | 10-12 | 9-12 | 9-12 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 |
5-7 |
Drying/Hr |
3-4 | 3-4 | 3-3.5 | 3 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 |
1.5-2 |
Detackifying/min |
5-8 | 5-8 | 5-8 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 8 |
8-15 |
Post exposure/min | 5-8 | 5-8 | 5-8 | 3-5 | 3-5 | 3-5 | 3-5 | 5 | 5 | 3-5 | 5 |
5 |
Specification of print plates typically for high-resolution |
||||||||
Model |
C284M-Ⅱ | C284H | C254-Ⅱ | C228LS | C170LS | C170H | C114LS | C114H |
Thickness/mm |
2.84 | 2.84 | 2.54 | 2.28 | 1.70 | 1.70 | 1.14 | 1.14 |
Hardness/Shore A | 53 | 58-60 | 56 | 56 | 62-64 | 70-72 | 69-71 |
75-76 |
Relief depth/mm | 1.0-1.4 | 1.0-1.4 | 1.0-1.2 | 1.0-1.2 | 0.7-0.9 | 0.7-0.9 | 0.6-0.7 |
0.6-0.7 |
Dot reproduction/% |
2-95% | 2-95% | 2-95% | 2-95% | 2-95% | 2-95% | 2-95% | 2-95% |
Line/lpi |
120 | 120 | 133 | 133 | 150 | 150 | 150 | 150 |
Isolated line/mm | 0.175 | 0.175 | 0.15 | 0.15 | 0.10 | 0.10 | 0.10 |
0.10 |
Isolated dot/mm | 0.25 | 0.25 | 0.20 | 0.20 | 0.20 | 0.20 | 0.20 |
0.20 |
Back Exposure/Sec |
25-40 | 25-40 | 25-40 | 35-55 | 25-40 | 15-21 | 35-60 | 35-70 |
Main Exposure/min |
8-20 | 8-20 | 8-15 | 8-20 | 10-18 | 10-18 | 10-18 | 10-18 |
Rinsing/min | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-7 |
5-7 |
Drying/Hr | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 | 1.5-2 |
1.5-2 |
Detackifying/min |
5-7 | 5-7 | 5-7 | 5-7 | 5-7 | 5-8 | 5-7 | 5-8 |
Post exposure/min | 5 | 5 | 5 | 5 | 5 | 5 | 5 |
5 |
Brands and Replacements |
|||||||||||
CorroGo OEM |
C700-Ⅱ | C635L | C550L | C470 | C394 | C394-Ⅱ | C394-Ⅲ | C394Q-Ⅱ | C318L | C284-Ⅱ | C284H |
Hardness (Shore A) |
36 | 36 | 36 | 36 | 43 | 43 | 38-36 | 42 | 37 | 46 | 58-60 |
DuPont Cyrel | / | HDC250 | / | / | HDC155 | HDC155 | DRC155 | HDC155 | / | NEOS112 |
/ |
Flint Nyloflex | / | / | / | / | / | ART155 | FAC155 | ART155 | FAC-X125 | ART112 |
ACE112 FAH112 |
Asahi AFP |
/ | / | / | / | / | / | SE3.94 | / | / | / | SH2.84 |
MacDermid | / | / | / | / | / | / | / | / | MGC125 | / |
MAX112 |
Brands and Replacements |
||||||||
CorroGo OEM |
C284M-Ⅱ | C284L | C254-Ⅱ | C228LS | C170LS | C170H | C114LS | C114H |
Hardness (Shore A) |
53 | 38-40 | 56 | 56 | 60-62 | 72 | 69-70 | 76 |
DuPont Cyrel | / | / | / | / | NEOS 67 | HIQS 67
NOWS67 |
NEOS 45 |
HIQS 45 NOWS45 |
Flint Nyloflex | FAR112
ACT112 |
FAC-X112 | FAR100
ACT100 |
FAR091 | FAR067
ACT067 |
FAH067
ACE067 |
FAR045
ACT045 |
FAH045 ACE045 |
Asahi AFP |
SF 2.84 | SE 2.84 | SF 2.54 | / | SF 1.7 | SH 1.7 | SF 1.14 | SH 1.14 |
MacDermid | MVP112 | MGC112 | MVP110 | / | MVP067 | MAX067 | MVP045 |
MAX045 |
Note: The above data sheet and results were tested with specific printing plate making equipment which may change due to different equipment, UV lamp, graphic depth and press requirements applied. The customer might test specifically to get optimized results.